Find suppliers for this alloy
C61200
| Elements | |||
|---|---|---|---|
| Cu | Fe | Al | |
| Min (%) | 7.0 | ||
| Max (%) | Rem | 0.05 | 9.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties