C61470
| Elements | |||||
|---|---|---|---|---|---|
| Cu | Pb | Fe | Al | Si | |
| Min (%) | 0.50 | 8.5 | |||
| Max (%) | Rem | 0.02 | 5.0 | 11.0 | 2.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties