C61600
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu | Sn | Zn | Fe | Ni | Al | Mn | Si | |
| Min (%) | 6.5 | |||||||
| Max (%) | Rem | 0.6 | 1.0 | 4.0 | 1.0 | 11.0 | 1.5 | 0.25 |