C61810
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu | Pb | Zn | Fe | Al | Si | |
| Min (%) | 0.50 | 8.5 | ||||
| Max (%) | Rem | 0.02 | 0.02 | 1.5 | 11.0 | 0.10 |