Find suppliers for this alloyC62500
Chemical Composition
Element
Cu(1,2)FeAlMn
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag.
Min (%)3.512.5
Max (%)Rem5.513.52.0
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell B scale
Shear Strength
(ksi)
Fatigue Strength**
(ksi)
BarAs Hot ExtrudedM30100   Typ
55   Typ
1   Typ
29   Typ
60   Typ
67   Typ
RodAs Hot ExtrudedM30100   Typ
55   Typ
1   Typ
29   Typ
60   Typ
67   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
Melting Point - Liquidus°F1925
Melting Point - Solidus°F1917
Densitylb/cu in. at 68°F0.26
Specific Gravity7.21
Electrical Conductivity% IACS at 68°F10
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F27
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi16000
Fabrication Properties
Technique Suitability
SolderingNot Recommended
BrazingFair
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingGood
Coated Metal Arc WeldingGood
Spot WeldFair
Seam WeldFair
Butt WeldFair
Capacity for Being Cold WorkedNot Recommended
Capacity for Being Hot FormedExcellent
Forgeability Rating80
Machinability Rating20
Common Fabrication Processes
  • Hot forging
  • Machining
    
Thermal Properties
Treatment Minimum* Maximum*
* Temperature is measured in Fahrenheit.
Annealing11001200
Hot Treatment13751550
Typical uses
Product Category Product Reason Category Reason
IndustrialBushingsBearing PropertiesLow Coefficient of Friction Mated with Steel
BushingsConductivity (Thermal)Thermal Conductivity
BushingsFriction & Wear PropertiesWear Resistance
BushingsMechanical PropertiesHigh Strength
CamsBearing PropertiesLow Coefficient of Friction Mated with Steel
CamsFriction & Wear PropertiesWear Resistance
CamsMechanical PropertiesHigh Strength
DiesBearing PropertiesLow Coefficient of Friction Mated with Steel
DiesConductivity (Thermal)High Thermal Conductivity
DiesFriction & Wear PropertiesWear Resistance
DiesMechanical PropertiesHigh Strength
Forming RollsBearing PropertiesLow Coefficient of Friction Mated with Steel
Forming RollsConductivity (Thermal)High Thermal Conductivity
Forming RollsFriction & Wear PropertiesWear Resistance
Forming RollsMechanical PropertiesHigh Strength
Guide BushingsBearing PropertiesLow Coefficient of Friction Mated with Steel
Guide BushingsFriction & Wear PropertiesWear Resistance
Guide BushingsMechanical PropertiesHigh Strength
Plastic Mold ComponentsBearing PropertiesLow Coefficient of Friction Mated with Steel
Plastic Mold ComponentsConductivity (Thermal)Thermal Conductivity
Plastic Mold ComponentsFriction & Wear PropertiesWear Resistance
Plastic Mold ComponentsMechanical PropertiesHigh Strength
Sheet Metal Forming DiesCorrosion ResistanceCorrosion Resistance
Sheet Metal Forming DiesFriction & Wear PropertiesWear Resistance
Sheet Metal Forming DiesMechanical PropertiesHigh Strength
Sheet Metal Forming DiesMechanical PropertiesRetains Strength at High Temperatures
Wear Plates for Plastic MoldsBearing PropertiesLow Coefficient of Friction Mated with Steel
Wear Plates for Plastic MoldsConductivity (Thermal)Thermal Conductivity
Wear Plates for Plastic MoldsFriction & Wear PropertiesWear Resistance
Wear Plates for Plastic MoldsMechanical PropertiesHigh Strength
Wear StripsBearing PropertiesLow Coefficient of Friction Mated with Steel
Wear StripsConductivity (Thermal)High Thermal Conductivity
Wear StripsFriction & Wear PropertiesWear Resistance
Wear StripsMechanical PropertiesHigh Strength
Welding RodConductivity (Electrical)Electrical Conductivity
Welding RodConductivity (Thermal)Thermal Conductivity
Welding RodCorrosion ResistanceOxidation Resistance
Welding RodSoftening ResistanceResistance to Thermal Softening
Wing Dies for Vertical Tube BendersBearing PropertiesLow Friction with Steel
Wing Dies for Vertical Tube BendersBearing PropertiesNon-Scratching
Wing Dies for Vertical Tube BendersFriction & Wear PropertiesWear Resistance
Wing Dies for Vertical Tube BendersOtherUsed on shorter runs than C
Applicable Specifications
Form Application System Standard Description
RodWeldingAWSA5.13SURFACE WELDING RODS AND ELECTRODES
Corrosion Properties

No information available.