C62730
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | Ni | Al | Mg | Mn | Si | |
| Min (%) | 4.0 | 4.0 | 8.5 | |||||||
| Max (%) | Rem | 0.05 | 0.10 | 0.40 | 6.0 | 6.0 | 11.0 | 0.05 | 0.05 | 0.10 |