C63020
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Co | Cr | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||||||
| Min (%) | 74.5 | 4.0 | 4.2 | 10.0 | ||||||
| Max (%) | 0.03 | 0.25 | 0.30 | 5.5 | 6.0 | 11.0 | 0.20 | 0.05 | 1.5 | |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Bearings | Corrosion Resistance | Corrosion Resistance |
| Bearings | Friction & Wear Properties | Resistant to Abrasive Wear | |
| Bearings | Friction & Wear Properties | Resistant to Adhesive Wear Toughness | |
| Bearings | Mechanical Properties | Heavy Load Strength | |
| Bushings | Corrosion Resistance | Corrosion Resistance | |
| Bushings | Mechanical Properties | Heavy Load Strength | |
| Bushings | Toughness | Resistance to Abrasive Wear | |
| Bushings | Toughness | Resistance to Adheasive Wear | |
| Forming Dies for Roll Bearings | Mechanical Properties | Heavy Duty | |
| Forming Dies for Roll Bearings | Mechanical Properties | High Mechanical Loading | |
| Forming Dies for Roll Bearings | Mechanical Properties | High Strength | |
| Hydraulic Bushings for Earth Moving Equipment | Corrosion Resistance | Corrosion Resistance | |
| Hydraulic Bushings for Earth Moving Equipment | Friction & Wear Properties | Resistant to Abrasive Wear | |
| Hydraulic Bushings for Earth Moving Equipment | Impact Resistance | Impact Resistant | |
| Hydraulic Bushings for Earth Moving Equipment | Mechanical Properties | High Strength | |
| Valve Balls | Corrosion Resistance | Cavitation Corrosion Resistance | |
| Valve Balls | Corrosion Resistance | Erosion Corrosion Resistance | |
| Valve Balls | Corrosion Resistance | Pitting Corrosion Resistance | |
| Valve Balls | Corrosion Resistance | Resistance to Corrosion by a broad variety of Corrosive Media | |
| Valve Balls | Finishing Characteristics | Retains Surface Finish | |
| Valve Balls | Friction & Wear Properties | Wear Resistance | |
| Valve Parts - Cryogenic | Corrosion Resistance | Corrosion Resistance | |
| Valve Parts - Cryogenic | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES | ||
| Pipe and Tube | Seamless | ASTM | B315 | SEAMLESS COPPER ALLOY PIPE AND TUBE | |
| Seamless | ASME | SB315 | COPPER-SILICON ALLOY SEAMLESS PIPE AND TUBE | ||
| Rod | ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES | ||
| Rod, Bar & Shapes | Aluminum Bronze | ASME | SB150 | ALUMINUM BRONZE ROD, BAR, AND SHAPES | |
| Shapes | AMS | 4590 | EXTRUSIONS, NICKEL-ALUMINUM BRONZE, MARTENSITIC, SOLUTION HEAT TREATED AND TEMPERED | ||
| ASTM | B150/B150M | ALUMINUM BRONZE ROD, BAR AND SHAPES |
Corrosion Properties