Find suppliers for this alloyC63020
Chemical Composition
Element
Cu(1,2)PbSnZnFeNi(3)AlCoCrMn
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co.
Min (%)74.54.04.210.0
Max (%)0.030.250.305.56.011.00.200.051.5
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialBearingsCorrosion ResistanceCorrosion Resistance
BearingsFriction & Wear PropertiesResistant to Abrasive Wear
BearingsFriction & Wear PropertiesResistant to Adhesive Wear Toughness
BearingsMechanical PropertiesHeavy Load Strength
BushingsCorrosion ResistanceCorrosion Resistance
BushingsMechanical PropertiesHeavy Load Strength
BushingsToughnessResistance to Abrasive Wear
BushingsToughnessResistance to Adheasive Wear
Forming Dies for Roll BearingsMechanical PropertiesHeavy Duty
Forming Dies for Roll BearingsMechanical PropertiesHigh Mechanical Loading
Forming Dies for Roll BearingsMechanical PropertiesHigh Strength
Hydraulic Bushings for Earth Moving EquipmentCorrosion ResistanceCorrosion Resistance
Hydraulic Bushings for Earth Moving EquipmentFriction & Wear PropertiesResistant to Abrasive Wear
Hydraulic Bushings for Earth Moving EquipmentImpact ResistanceImpact Resistant
Hydraulic Bushings for Earth Moving EquipmentMechanical PropertiesHigh Strength
Valve BallsCorrosion ResistanceCavitation Corrosion Resistance
Valve BallsCorrosion ResistanceErosion Corrosion Resistance
Valve BallsCorrosion ResistancePitting Corrosion Resistance
Valve BallsCorrosion ResistanceResistance to Corrosion by a broad variety of Corrosive Media
Valve BallsFinishing CharacteristicsRetains Surface Finish
Valve BallsFriction & Wear PropertiesWear Resistance
Valve Parts - CryogenicCorrosion ResistanceCorrosion Resistance
Valve Parts - CryogenicMechanical PropertiesHigh Strength
Applicable Specifications
Form System Standard Description
BarASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
PipeASTMB315SEAMLESS COPPER ALLOY PIPE AND TUBE
RodASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
ShapesAMS4590EXTRUSIONS, NICKEL-ALUMINUM BRONZE, MARTENSITIC, SOLUTION HEAT TREATED AND TEMPERED
ASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
TubeASTMB315SEAMLESS COPPER ALLOY PIPE AND TUBE
Corrosion Properties

No information available.