Find suppliers for this alloy
C63230
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu | Pb | Fe | Ni | Al | Mn | Si | |
| Min (%) | 75.9 | 3.0 | 4.0 | 8.5 | |||
| Max (%) | 84.4 | 0.02 | 5.0 | 5.5 | 9.5 | 3.5 | 0.10 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties