C63280
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Fe | Ni(3) | Al | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||
| Min (%) | 3.0 | 4.0 | 8.5 | 0.6 | ||
| Max (%) | Rem | 0.02 | 5.0 | 5.5 | 9.5 | 3.5 |