Find suppliers for this alloy
C63300
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu | Pb | Fe | Ni | Al | Mn | Si | |
| Min (%) | 2.0 | 1.0 | 5.0 | 11.0 | |||
| Max (%) | Rem | 0.02 | 6.0 | 2.5 | 7.5 | 13.0 | 1.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Welding Rod | Conductivity (Electrical) | Electrical Conductivity |
| Welding Rod | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Rod | Corrosion Resistance | Oxidation Resistance | |
| Welding Rod | Softening Resistance | Resistance to Thermal Softening |
Applicable Specifications
Corrosion Properties