C63400
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | As | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
|||||||||
| Min (%) | 2.6 | 0.25 | |||||||
| Max (%) | Rem | 0.05 | 0.20 | 0.50 | 0.15 | 0.15 | 3.2 | 0.09 | 0.45 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Pole Line Hardware | Corrosion Resistance | Corrosion Resistance |
| Pole Line Hardware | Corrosion Resistance | Stress Corrosion Cracking Resistance | |
| Pole Line Hardware | Mechanical Properties | High Strength | |
| Fasteners | Fasteners | Corrosion Resistance | Corrosion Resistance |
| Fasteners | Corrosion Resistance | Stress Corrosion Cracking Resistance | |
| Fasteners | Mechanical Properties | High Strength |
Applicable Specifications
Corrosion Properties