Find suppliers for this alloy
C63500
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Sn | Zn | Fe | Al | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. |
|||||
| Min (%) | 0.50 | 4.5 | 0.15 | 4.5 | |
| Max (%) | Rem | 2.0 | 7.0 | 0.50 | 7.0 |
Mechanical Properties
| Melting Point - Liquidus°F | 1886 |
|---|---|
| Melting Point - Solidus°F | 1832 |
| Densitylb/cu in. at 68°F | 0.296 |
| Electrical Conductivity% IACS at 68°F | 15.4 |
| Modulus of Elasticity in Tensionksi | 18900 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Poor |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties