Find suppliers for this alloyC63500
Chemical Composition
Element
Cu(1,2)SnZnFeAl
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min.
Min (%)0.504.50.154.5
Max (%)Rem2.07.00.507.0
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Melting Point - Liquidus°F1886
Melting Point - Solidus°F1832
Densitylb/cu in. at 68°F0.296
Electrical Conductivity% IACS at 68°F15.4
Modulus of Elasticity in Tensionksi18900
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Capacity for Being Cold WorkedGood
Capacity for Being Hot FormedPoor
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
OtherMedical Equipment
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.