Find suppliers for this alloy
C63600
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | As | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||||
| Min (%) | 3.0 | 0.7 | |||||||
| Max (%) | Rem | 0.05 | 0.20 | 0.50 | 0.15 | 0.15 | 4.0 | 0.15 | 1.3 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
Rockwell B scale | Section Size (in) |
Cold Work (%) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Rod | 1/4 Hard | H01 |
74 Typ |
31 Typ |
0.55 | ||
| Annealed | O61 |
60 Typ |
64 Typ |
||||
| Wire | 1/4 Hard | H01 |
84 Typ |
29 Typ |
84 Typ |
0.488 | 21 |
| 1/8 Hard | H00 |
68 Typ |
52 Typ |
71 Typ |
0.422 | 7 | |
| Annealed | O61 |
60 Typ |
67 Typ |
0.392 | |||
| Melting Point - Liquidus°F | 1890 |
|---|---|
| Densitylb/cu in. at 68°F | 0.301 |
| Specific Gravity | 8.33 |
| Electrical Conductivity% IACS at 68°F | 12 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 33 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.4 |
| Modulus of Elasticity in Tensionksi | 16000 |
| Technique | Suitability |
|---|---|
| Soldering | Not Recommended |
| Brazing | Not Recommended |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Fair |
| Seam Weld | Fair |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Fair |
| Machinability Rating | 40 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Hot Working Temperature | 1400 | 1600 | ||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Cable Connectors | Conductivity (Electrical) | Electrical Conductivity |
| Cable Connectors | Conductivity (Thermal) | High Thermal Conductivity | |
| Cable Connectors | Corrosion Resistance | Corrosion Resistance | |
| Cable Connectors | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Cable Connectors | Mechanical Properties | High Strength | |
| Cold Headed Nuts | Conductivity (Electrical) | Electrical Conductivity | |
| Cold Headed Nuts | Conductivity (Thermal) | High Thermal Conductivity | |
| Cold Headed Nuts | Corrosion Resistance | Corrosion Resistance | |
| Cold Headed Nuts | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Components for Pole Line Hardware | Conductivity (Electrical) | Electrical Conductivity | |
| Components for Pole Line Hardware | Conductivity (Thermal) | High Thermal Conductivity | |
| Components for Pole Line Hardware | Corrosion Resistance | Corrosion Resistance | |
| Components for Pole Line Hardware | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Components for Pole Line Hardware | Machining Properties | Machinability, Good | |
| Components for Pole Line Hardware | Mechanical Properties | High Strength | |
| Fasteners | Bolts | Corrosion Resistance | Corrosion Resistance |
| Bolts | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Bolts | Mechanical Properties | High Strength | |
| Screw Machine Products | Corrosion Resistance | Corrosion Resistance | |
| Screw Machine Products | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Screw Machine Products | Mechanical Properties | Moderate Strength | |
| Industrial | Valve Components, Nuclear Power Service | Corrosion Resistance | Corrosion Resistance to Uranium Hexafloride |
| Valve Components, Nuclear Power Service | Forging Characteristics | Forgability | |
| Valve Components, Nuclear Power Service | Mechanical Properties | Moderate Strength |
Applicable Specifications
Corrosion Properties