Find suppliers for this alloyC64210
Chemical Composition
Element
Cu(1,2)PbSnZnFeNi(3)AlAsMnSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co.
Min (%)6.31.5
Max (%)Rem0.050.200.500.300.257.00.090.102.0
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Densitylb/cu in. at 68°F0.278
Specific Gravity7.7
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalPole Line HardwareConductivity (Electrical)Electrical Conductivity
Pole Line HardwareConductivity (Thermal)Thermal Conductivity
Pole Line HardwareCorrosion ResistanceCorrosion Resistance
Pole Line HardwareMechanical PropertiesHigh Strength
IndustrialBearings, High Strength, Corrosion ResistantCorrosion ResistanceCorrosion Resistance
Bearings, High Strength, Corrosion ResistantCorrosion ResistanceCorrosion Resistance to Numerous Environments
Bearings, High Strength, Corrosion ResistantFriction & Wear PropertiesWear Resistance
Bearings, High Strength, Corrosion ResistantMachining CharacteristicsMachinability, Good
Bearings, High Strength, Corrosion ResistantMechanical PropertiesHigh Strength
Bushings, AircraftCorrosion ResistanceCorrosion Resistance
Bushings, AircraftCorrosion ResistanceCorrosion Resistance to Numerous Environments
Bushings, AircraftCorrosion ResistanceCorrosion Resistance to the Atmosphere
Bushings, AircraftMachining CharacteristicsMachinability, Good
Bushings, AircraftMechanical PropertiesHigh Strength
Chemical Process EquipmentCorrosion ResistanceCorrosion Resistance
Chemical Process EquipmentCorrosion ResistanceCorrosion Resistance to Acids
Chemical Process EquipmentCorrosion ResistanceCorrosion Resistance to Numerous Environments
Chemical Process EquipmentMechanical PropertiesHigh Strength
Pickling EquipmentCorrosion ResistanceCorrosion Resistance
Pickling EquipmentCorrosion ResistanceCorrosion Resistance to Acids
Pickling EquipmentCorrosion ResistanceCorrosion Resistance to Numerous Environments
Pickling EquipmentMechanical PropertiesHigh Strength
Valve BodiesCorrosion ResistanceCorrosion Resistance
Valve BodiesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Valve BodiesFriction & Wear PropertiesWear Resistance
Valve BodiesMachining CharacteristicsMachinability, Good
Valve BodiesMechanical PropertiesHigh Strength
Valve StemsCorrosion ResistanceCorrosion Resistance
Valve StemsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Valve StemsFriction & Wear PropertiesWear Resistance
Valve StemsMachining PropertiesMachinability, Good
Valve StemsMechanical PropertiesHigh Strength
MarineBoltsCorrosion ResistanceCorrosion Resistance
BoltsCorrosion ResistanceCorrosion Resistance to Numerous Environments
BoltsMachining PropertiesMachinability, Good
BoltsMechanical PropertiesHigh Strength
Lock washersCorrosion ResistanceCorrosion Resistance
Lock washersCorrosion ResistanceCorrosion Resistance to Numerous Environments
Lock washersMachining PropertiesMachinability, Good
Lock washersMechanical PropertiesHigh Strength
NutsCorrosion ResistanceCorrosion Resistance
NutsCorrosion ResistanceCorrosion Resistance to Numerous Environments
NutsMachining PropertiesMachinability, Good
NutsMechanical PropertiesHigh Strength
ScrewsCorrosion ResistanceCorrosion Resistance
ScrewsCorrosion ResistanceCorrosion Resistance to Numerous Environments
ScrewsMachining PropertiesMachinability, Good
ScrewsMechanical PropertiesHigh Strength
Applicable Specifications
Form Sub-Form System Standard Description
BarASTMB124/B1124MCOPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES
ASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
DieForgingsASTMB283/B283MCOPPER AND COPPER ALLOY DIE FORGINGS (HOT PRESSED)
RodASTMB124/B1124MCOPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES
ASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
ShapesForgingsASTMB124/B1124MCOPPER AND COPPER-ALLOY FORGING ROD, BAR AND SHAPES
ASTMB150/B150MALUMINUM BRONZE ROD, BAR AND SHAPES
Corrosion Properties