Find suppliers for this alloy
C64710
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Zn | Ni(3) | Mn | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||
| Min (%) | 95.0 | 0.20 | 2.9 | 0.50 | |
| Max (%) | 0.50 | 3.5 | 0.10 | 0.9 | |