| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Ca | Cr | Mg | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||||||
| Min (%) | 0.20 | 0.20 | 2.5 | 0.002 | 0.50 | |||||
| Max (%) | Rem | 0.01 | 0.8 | 1.0 | 0.25 | 3.0 | 0.01 | 0.01 | 0.20 | 0.8 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | Precipitation or Spinodal Heat-treated, 1/4 Hard and Thermal Stress Relieved | TR01 |
96 Min 138 Max |
77 Min 138 Max |
1 Min |
170 Min 290 Max |
| Melting Point - Liquidus°F | 1985 |
|---|---|
| Melting Point - Solidus°F | 1920 |
| Densitylb/cu in. at 68°F | 0.32 |
| Specific Gravity | 8.87 |
| Electrical Conductivity% IACS at 68°F | 40 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 102 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 95 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 19200 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Fair |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Good |
| Seam Weld | Good |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
| Forgeability Rating | 70 |
| Machinability Rating | 20 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 660 | 1200 | ||
| Hot Working Temperature | 1557 | 1755 | ||