| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
|||||||
| Min (%) | 0.10 | 0.10 | 2.0 | 0.30 | |||
| Max (%) | Rem | 0.05 | 1.0 | 2.0 | 0.20 | 3.6 | 0.9 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| Flat Products | Hard | H04 |
110 Min 120 Typ 130 Max |
105 Min 115 Typ 125 Max |
| Melting Point - Liquidus°F | 1913 |
|---|---|
| Melting Point - Solidus°F | 1868 |
| Densitylb/cu in. at 68°F | 0.321 |
| Specific Gravity | 8.87 |
| Electrical Conductivity% IACS at 68°F | 41 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 95 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.7 |
| Modulus of Elasticity in Tensionksi | 18400 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Fair |
Common Fabrication Processes