C64745
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co. |
||||||||
| Min (%) | 0.20 | 0.20 | 0.7 | 0.10 | ||||
| Max (%) | Rem | 0.05 | 0.80 | 0.8 | 0.20 | 2.5 | 0.10 | 0.7 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Flat Products | Extra Hard | H06 |
106 Typ |
104 Typ |
3 Min |
Physical Properties
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Spot Weld | Excellent |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Excellent |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties