Find suppliers for this alloy
C64785
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Not including Co. |
||||||||||
| Min (%) | 0.50 | 3.0 | 0.40 | 3.0 | 0.20 | |||||
| Max (%) | Rem | 0.015 | 2.0 | 6.0 | 0.02 | 0.015 | 1.6 | 6.0 | 1.0 | 0.15 |
Mechanical Properties
| Melting Point - Solidus°F | 1915 |
|---|---|
| Densitylb/cu in. at 68°F | 0.293 |
| Specific Gravity | 8.11 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet & Strip | Copper Clad Stainless | ASTM | B694 | COPPER, COPPER ALLOY AND COPPER-CLAD STAINLESS STEEL SHEET AND STRIP FOR ELECTRICAL CABLE SHIELDING |
Corrosion Properties