Find suppliers for this alloyC64785
Chemical Composition
Element
Cu(1,2)PbSnZnFePNi(3)AlMnSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Not including Co.
Min (%)0.503.00.403.00.20
Max (%)Rem0.0152.06.00.020.0151.66.01.00.15
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Melting Point - Solidus°F1915
Densitylb/cu in. at 68°F0.293
Specific Gravity8.11
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialClad Products
Applicable Specifications
Form Sub-Form System Standard Description
Sheet & StripCopper Clad Stainless ASTMB694COPPER, COPPER ALLOY AND COPPER-CLAD STAINLESS STEEL SHEET AND STRIP FOR ELECTRICAL CABLE SHIELDING
Corrosion Properties

No information available.