Find suppliers for this alloy
							
							
								
									C64800 
									
								
								
									
									
										
							  
							    
							
							  
							    
							
							  
							    
							
							  
							    
							
								
									
	| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni | Co | Cr | Si | |
| 
												(1) Cu + Sum of Named Elements 99.5% min.   (2) Cu value includes Ag.  | 
										||||||||||
| Min (%) | 1.0 | 0.20 | ||||||||
| Max (%) | Rem | 0.05 | 0.50 | 0.50 | 1.0 | 0.50 | 0.50 | 3.0 | 0.09 | 1.0 | 
| Form | Temper | Temper Code | Tensile Strength (ksi)  | 
							        YS-0.2% Offset (ksi)  | 
							        
							        
											
											Elongation (%)  | 
											
							        
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
							      
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Flat Products | Hard | H04 | 
												83 Min 97 Typ 104 Max  | 
											80 Min 94 Typ 102 Max  | 
											
											
											
											8 Typ | 
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
											
							      
| Densitylb/cu in. at 68°F | 0.32 | 
|---|---|
| Specific Gravity | 8.85 | 
| Electrical Conductivity% IACS at 68°F | 65 | 
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 150 | 
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.9 | 
| Modulus of Elasticity in Tensionksi | 18400 | 
| Technique | Suitability | 
|---|---|
| Capacity for Being Cold Worked | Good | 
| Capacity for Being Hot Formed | Fair | 
							  Common Fabrication Processes
							  
							
							  Thermal Properties
								  
							
							  Typical Uses
							  
							
							  Applicable Specifications
							  
							
								Corrosion Properties