Find suppliers for this alloyC64800
Chemical Composition
Element
Cu(1,2)PbSnZnFePNiCoCrSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag.
Min (%)1.00.20
Max (%)Rem0.050.500.501.00.500.503.00.091.0
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Flat ProductsHardH0483   Min
97   Typ
104   Max
80   Min
94   Typ
102   Max
8   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Densitylb/cu in. at 68°F0.32
Specific Gravity8.85
Electrical Conductivity% IACS at 68°F65
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F150
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.9
Modulus of Elasticity in Tensionksi18400
Fabrication Properties
Technique Suitability
Capacity for Being Cold WorkedGood
Capacity for Being Hot FormedFair
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalConnectors
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.