Find suppliers for this alloy
C64810
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Co | Cr | Mg | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||||
| Min (%) | 0.10 | 0.50 | 0.20 | ||||||||
| Max (%) | Rem | 0.05 | 0.50 | 0.50 | 1.0 | 0.50 | 1.0 | 3.0 | 0.09 | 0.20 | 1.0 |
| Form | Temper | Temper Code | YS-0.2% Offset (ksi) |
Elongation (%) |
Ultimate Tensile Strength in Shear (ksi) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Sheet | Extra Hard | H06 | 94 Min 109 Typ 123 Max |
3 Typ |
99 Min 113 Typ 128 Max |
| Densitylb/cu in. at 68°F | 0.32 |
|---|---|
| Specific Gravity | 8.86 |
| Electrical Conductivity% IACS at 68°F | 60 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 142 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.8 |
| Modulus of Elasticity in Tensionksi | 17400 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Capacity for Being Cold Worked | Excellent |
| Capacity for Being Hot Formed | Good |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties