Find suppliers for this alloyC64810
Chemical Composition
Element
Cu(1)PbSnZnFePNiCoCrMgSi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)0.100.500.20
Max (%)Rem0.050.500.501.00.501.03.00.090.201.0
Mechanical Properties*
Form
Temper
Temper Code
YS-0.2% Offset
Elongation
(%)
Ultimate Tensile Strength in Shear
(ksi)
SheetExtra HardH0694   Min
109   Typ
123   Max
3   Typ
99   Min
113   Typ
128   Max
* Measured at room temperature, 68°F (20°C).
Physical Properties
Densitylb/cu in. at 68°F0.32
Specific Gravity8.86
Electrical Conductivity% IACS at 68°F60
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F142
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)9.8
Modulus of Elasticity in Tensionksi17400
Fabrication Properties
Technique Suitability
SolderingGood
Capacity for Being Cold WorkedExcellent
Capacity for Being Hot FormedGood
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalElectrical Connectors
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.