Find suppliers for this alloy
C64850
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1) | Fe | P | Ni | Co | Mg | Mn | Si | |
|
(1) Cu + Sum of Named Elements, 99.95% min. |
||||||||
| Min (%) | 0.05 | 0.001 | 1.2 | 0.20 | ||||
| Max (%) | Rem | 0.50 | 0.05 | 0.05 | 2.5 | 0.05 | 0.05 | 1.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Vickers Hardness, 3000 gm |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Sheet & Strip | Hard | H04 |
85.6 Min 104.4 Max |
78.3 Min 97.2 Max |
180 Typ |
| Melting Point - Liquidus°F | 1973 |
|---|---|
| Melting Point - Solidus°F | 1982 |
| Densitylb/cu in. at 68°F | 0.32 |
| Specific Gravity | 8.85 |
| Electrical Conductivity% IACS at 68°F | 65 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 150 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10.3 |
| Modulus of Elasticity in Tensionksi | 12700 |
| Poisson's Ratio | 0.33 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties