Find suppliers for this alloy
C65600
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Al | Mn | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. |
||||||||
| Min (%) | 2.8 | |||||||
| Max (%) | Rem | 0.02 | 1.5 | 1.5 | 0.50 | 0.01 | 1.5 | 4.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Welding Rod, Filler Metal | Brazing Characteristics | Fluidity |
| Welding Rod, Filler Metal | Conductivity (Electrical) | Electrical Conductivity | |
| Welding Rod, Filler Metal | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Rod, Filler Metal | Mechanical Properties | Moderate to High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Electrode | Welding | AWS | A5.6 | COPPER AND COPPER ALLOY COVERED ELECTRODES | |
| Rod | Welding | AWS | A5.7 | COPPER AND COPPER ALLOY BARS, WELDING RODS | |
| Welding | AWS | A5.27 | COPPER AND COPPER ALLOY RODS FOR OXYFUEL GAS WELDING |
Corrosion Properties