Find suppliers for this alloy
C65620
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Zn | Fe | P | Mn | Si | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 90.0 | 1.5 | 1.0 | 2.4 | ||
| Max (%) | 4.0 | 2.0 | 0.10 | 1.0 | 4.0 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Forgings |
56 Typ |
20 Typ |
30 Typ |
55 Typ |
||
| Rod & Bar |
56 Typ |
20 Typ |
30 Typ |
55 Typ |
||
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bar | AMS | 4616 | SILICON BRONZE BARS, RODS, FORGINGS AND TUBING, STRESS RELIEVED | ||
| Forgings | AMS | 4616 | SILICON BRONZE BARS, RODS, FORGINGS AND TUBING, STRESS RELIEVED | ||
| Rod | AMS | 4616 | SILICON BRONZE BARS, RODS, FORGINGS AND TUBING, STRESS RELIEVED | ||
| Tube | AMS | 4616 | SILICON BRONZE BARS, RODS, FORGINGS AND TUBING, STRESS RELIEVED |
Corrosion Properties