C65800
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Fe | Ni | Mn | Si | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 0.50 | 2.5 | ||||
| Max (%) | Rem | 0.05 | 0.25 | 0.6 | 1.3 | 3.8 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.308 |
|---|---|
| Specific Gravity | 8.53 |