C66100
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||
| Min (%) | 0.20 | 2.8 | ||||
| Max (%) | Rem | 0.8 | 1.5 | 0.25 | 1.5 | 3.5 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.308 |
|---|---|
| Specific Gravity | 8.53 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Contact springs | Conductivity (Electrical) | Electrical Conductivity |
| Contact springs | Conductivity (Thermal) | Thermal Conductivity | |
| Contact springs | Corrosion Resistance | Corrosion Resistance | |
| Contact springs | Forming Characteristics | Formability | |
| Contact springs | Mechanical Properties | High Modulus of Elasticity | |
| Contact springs | Mechanical Properties | Moderate Strength | |
| Contacts | Conductivity (Electrical) | Electrical Conductivity | |
| Contacts | Conductivity (Thermal) | Thermal Conductivity | |
| Contacts | Corrosion Resistance | Corrosion Resistance | |
| Contacts | Forming Characteristics | Formability | |
| Contacts | Mechanical Properties | Moderate Strength | |
| Sockets | Conductivity (Electrical) | Electrical Conductivity | |
| Sockets | Conductivity (Thermal) | Thermal Conductivity | |
| Sockets | Corrosion Resistance | Corrosion Resistance | |
| Sockets | Forming Characteristics | Formability | |
| Sockets | Mechanical Properties | Moderate Strength | |
| Switch blades | Conductivity (Electrical) | Electrical Conductivity | |
| Switch blades | Conductivity (Thermal) | Thermal Conductivity | |
| Switch blades | Corrosion Resistance | Corrosion Resistance | |
| Switch blades | Forming Characteristics | Formability | |
| Switch blades | Mechanical Properties | High Modulus of Elasticity | |
| Switch blades | Mechanical Properties | Moderate Strength | |
| Terminals | Conductivity (Electrical) | Electrical Conductivity | |
| Terminals | Conductivity (Thermal) | Thermal Conductivity | |
| Terminals | Corrosion Resistance | Corrosion Resistance | |
| Terminals | Forming Characteristics | Formability | |
| Terminals | Mechanical Properties | High Modulus of Elasticity | |
| Terminals | Mechanical Properties | Moderate Strength | |
| Industrial | Bearings | Corrosion Resistance | Corrosion Resistance |
| Bearings | Friction & Wear Properties | Galling Resistance | |
| Bearings | Machining Characteristics | Machinability | |
| Bearings | Mechanical Properties | Moderate toHigh Strength | |
| Bushings | Corrosion Resistance | Corrosion Resistance | |
| Bushings | Friction & Wear Properties | Galling Resistance | |
| Bushings | Machining Characteristics | Machinability | |
| Bushings | Mechanical Properties | Moderate to High Strength | |
| High Speed Screw Mahcine Products | Machining Characteristics | Screw Machinability | |
| High Strength Bolts | Mechanical Properties | High Strength | |
| Oil Refinery Plumbing Tube | Corrosion Resistance | Corrosion Resistance | |
| Oil Refinery Plumbing Tube | Corrosion Resistance | Corrosion Resistance to Petrochemicals | |
| Oil Refinery Plumbing Tube | Machining Characteristics | Machinability | |
| Oil Refinery Plumbing Tube | Mechanical Properties | Fatigue Resistance | |
| Oil Refinery Plumbing Tube | Mechanical Properties | Moderate Strength | |
| Oil Refinery Plumbing Tube | Non-Sparking | Non-Sparking | |
| Oil Refinery Plumbing Tube | Welding Characteristics | Weldability | |
| Pole Hardware | Fouling Resistance | Anti-Fouling | |
| Pole Hardware | Mechanical Properties | Strength | |
| Marine | Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Bolts | ASTM | F468 | NONFERROUS BOLTS, HEX CAP SCREWS, AND STUDS FOR GENERAL USE | ||
| Nuts | ASTM | F467 | NONFERROUS NUTS FOR GENERAL USE | ||
| Rod, Bar & Shapes | Copper-Silicon Alloy | ASTM | B98/B98M | COPPER-SILICON ALLOY ROD, BAR AND SHAPES | |
| Copper-Silicon Alloy | ASME | SB98 | COPPER-SILICON ALLOY ROD, BAR AND SHAPES | ||
| Screws | ASTM | F468 | NONFERROUS BOLTS, HEX CAP SCREWS, AND STUDS FOR GENERAL USE | ||
| Studs | ASTM | F468 | NONFERROUS BOLTS, HEX CAP SCREWS, AND STUDS FOR GENERAL USE |
Corrosion Properties