C66300
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe(3) | P | Co(4) | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Fe + Co, 1.4 - 2.4% (4) Fe + Co, 1.4 - 2.4% |
|||||||
| Min (%) | 84.5 | 1.5 | 1.4 | ||||
| Max (%) | 87.5 | 0.05 | 3.0 | Rem | 2.4 | 0.35 | 0.20 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Section Size (in) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | Anneal to Temper - 1/2 Hard | O82 |
66 Typ |
58 Typ |
20 Min |
0.1 |
| Extra Hard | H06 |
96 Typ |
94 Typ |
7 Typ |
0.089 | |
| Extra Spring | H10 |
107 Typ |
106 Typ |
5 Typ |
0.075 | |
| Extra Spring and Stress Relieved | HR10 |
107 Typ |
105 Typ |
2 Min |
0.075 | |
| Hard | H04 |
84 Typ |
81 Typ |
17 Typ |
0.166 | |
| Hard and Stress Relieved | HR04 |
84 Typ |
80 Typ |
9 Min |
0.116 | |
| Spring | H08 |
103 Typ |
100 Typ |
6 Typ |
0.075 | |
| Spring and Stress Relieved | HR08 |
103 Typ |
100 Typ |
4 Min |
0.075 | |
| Super Spring | H14 |
105 Min |
105 Min |
5 Max | 0.067 | |
| Melting Point - Liquidus°F | 1920 |
|---|---|
| Melting Point - Solidus°F | 1830 |
| Densitylb/cu in. at 68°F | 0.317 |
| Specific Gravity | 8.78 |
| Electrical Conductivity% IACS at 68°F | 25 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 62 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 9.4 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 9.8 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 9.9 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 18000 |
| Modulus of Rigidityksi | 6900 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Clutch discs | Conductivity (Thermal) | Thermal Conductivity |
| Clutch discs | Friction & Wear Properties | Abrasion Resistance | |
| Clutch discs | Friction & Wear Properties | Wear Resistance | |
| Clutch discs | Mechanical Properties | Strength | |
| Bearings | Bushings, sleeve | Bearing Properties | Abrasion Resistance |
| Bushings, sleeve | Friction & Wear Properties | Wear Resistance | |
| Electrical | Connectors | Conductivity (Electrical) | Electrical Conductivity |
| Connectors | Forming Characteristics | Excellent Formability | |
| Connectors | Mechanical Properties | Moderate Strength | |
| Connectors | Thermal Properties | Resistance to Stress Relaxation | |
| Fuse Clips | Forming Characteristics | Formability | |
| Fuse Clips | Mechanical Properties | Strength | |
| Switch Gear | Conductivity (Electrical) | Electrical Conductivity | |
| Switch Gear | Friction & Wear Properties | Wear Resistance | |
| Switch Gear | Machining Characteristics | Machinability | |
| Switch Gear | Mechanical Properties | Strength | |
| Terminals | Conductivity (Electrical) | Electrical Conductivity | |
| Terminals | Mechanical Properties | Ductility | |
| Terminals | Solderability | Solderability | |
| Fasteners | Fasteners | Conductivity (Electrical) | Electrical Conductivity |
| Fasteners | Forming Characteristics | Formability | |
| Lock Washers | Conductivity (Electrical) | Electrical Conductivity | |
| Lock Washers | Forming Characteristics | Formability | |
| Hardware | Beater bars | Drawing Characteristics | Drawability |
| Beater bars | Mechanical Properties | Ductility | |
| Beater bars | Mechanical Properties | Fatigue Strength | |
| Bellows | Drawing Characteristics | Capacity for Cold Drawing | |
| Bellows | Non-Fouling | Fatigue Life | |
| Diaphrams | Mechanical Properties | Ductility | |
| Diaphrams | Mechanical Properties | Strength | |
| Diaphrams | Stress Relaxation | Stress Relaxation Resistance | |
| Springs | Mechanical Properties | Ductility | |
| Springs | Mechanical Properties | Stiffness | |
| Springs | Mechanical Properties | Strength | |
| Industrial | Bridge bearing plates | Friction & Wear Properties | Abrasion Resistance |
| Bridge bearing plates | Friction & Wear Properties | Wear Resistance | |
| Chemical hardware | Corrosion Resistance | Corrosion Resistance | |
| Chemical hardware | Mechanical Properties | Strength | |
| Perferated sheets | Appearance | Color | |
| Textile machinery | Friction & Wear Properties | Wear Resistance | |
| Textile machinery | Mechanical Properties | Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet, Strip, Roller Bar & Plate | ASTM | B592 | COPPER-ZINC-ALUMINUM-COBALT ALLOY PLATE, SHEET, STRIP, AND ROLLED BAR |
Corrosion Properties