Find suppliers for this alloy
C66410
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. |
|||||
| Min (%) | 11.0 | 1.8 | |||
| Max (%) | Rem | 0.015 | 0.05 | 12.0 | 2.3 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Sheet | ASTM | B694 | COPPER, COPPER ALLOY AND COPPER-CLAD STAINLESS STEEL SHEET AND STRIP FOR ELECTRICAL CABLE SHIELDING | ||
| Strip | ASTM | B694 | COPPER, COPPER ALLOY AND COPPER-CLAD STAINLESS STEEL SHEET AND STRIP FOR ELECTRICAL CABLE SHIELDING |
Corrosion Properties