Find suppliers for this alloy
C66500
| Elements | |||||
|---|---|---|---|---|---|
| Cu(1) | Pb | Zn | Fe | Mn | |
|
(1) Cu value includes Ag. |
|||||
| Min (%) | 80.0 | 0.7 | |||
| Max (%) | 82.0 | 0.05 | Rem | 0.10 | 1.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties