C66800
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||||
| Min (%) | 60.0 | 2.0 | 0.50 | ||||||
| Max (%) | 63.0 | 0.50 | 0.30 | Rem | 0.35 | 0.25 | 0.25 | 3.5 | 1.5 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Bearings | Corrosion Resistance | Corrosion Resistance |
| Bearings | Forming Characteristics | Formability | |
| Bearings | Friction & Wear Properties | Wear Resistance | |
| Bearings | Mechanical Properties | Ductility | |
| Bearings | Mechanical Properties | Moderate Strength | |
| Bushings | Corrosion Resistance | Corrosion Resistance | |
| Bushings | Forming Characteristics | Formability | |
| Bushings | Friction & Wear Properties | Wear Resistance | |
| Bushings | Mechanical Properties | Ductility | |
| Bushings | Mechanical Properties | Moderate Strength | |
| Cams | Corrosion Resistance | Corrosion Resistance | |
| Cams | Forming Characteristics | Formability | |
| Cams | Friction & Wear Properties | Wear Resistance | |
| Cams | Mechanical Properties | Ductility | |
| Cams | Mechanical Properties | Moderate Strength | |
| Connecting Rods | Corrosion Resistance | Corrosion Resistance | |
| Connecting Rods | Mechanical Properties | Ductility | |
| Connecting Rods | Mechanical Properties | High Strength | |
| Connecting Rods | Welding Characteristics | Weldability | |
| Drive Shafts | Corrosion Resistance | Corrosion Resistance | |
| Drive Shafts | Mechanical Properties | Ductility | |
| Drive Shafts | Mechanical Properties | High Strength | |
| Gears | Corrosion Resistance | Corrosion Resistance | |
| Gears | Forming Characteristics | Formability | |
| Gears | Friction & Wear Properties | Wear Resistance | |
| Gears | Mechanical Properties | Ductility | |
| Gears | Mechanical Properties | Moderate Strength | |
| Idler Pins | Corrosion Resistance | Corrosion Resistance | |
| Idler Pins | Forming Characteristics | Formability | |
| Idler Pins | Mechanical Properties | Ductility | |
| Idler Pins | Mechanical Properties | High Strength | |
| Piston Heads | Corrosion Resistance | Corrosion Resistance | |
| Piston Heads | Forming Characteristics | Formability | |
| Piston Heads | Friction & Wear Properties | Wear Resistance | |
| Piston Heads | Mechanical Properties | Ductility | |
| Piston Heads | Mechanical Properties | High Strength | |
| Piston Heads | Pressure Tight | Pressure Tight | |
| Sealing Rings | Corrosion Resistance | Corrosion Resistance | |
| Sealing Rings | Mechanical Properties | Ductility | |
| Sealing Rings | Mechanical Properties | High Strength | |
| Sealing Rings | Pressure Tight | Pressure Tight | |
| Sleeve Bearings | Corrosion Resistance | Corrosion Resistance | |
| Sleeve Bearings | Forming Characteristics | Formability | |
| Sleeve Bearings | Friction & Wear Properties | Wear Resistance | |
| Sleeve Bearings | Mechanical Properties | Ductility | |
| Sleeve Bearings | Mechanical Properties | High Strength | |
| Spindles | Corrosion Resistance | Corrosion Resistance | |
| Spindles | Forming Characteristics | Formability | |
| Spindles | Mechanical Properties | Ductility | |
| Spindles | Mechanical Properties | High Strength | |
| Thrust Bearings | Corrosion Resistance | Corrosion Resistance | |
| Thrust Bearings | Forming Characteristics | Formability | |
| Thrust Bearings | Friction & Wear Properties | Wear Resistance | |
| Thrust Bearings | Mechanical Properties | Ductility | |
| Thrust Bearings | Mechanical Properties | High Strength | |
| Valve Seats | Corrosion Resistance | Corrosion Resistance | |
| Valve Seats | Friction & Wear Properties | Wear Resistance | |
| Valve Seats | Mechanical Properties | Ductility | |
| Valve Seats | Mechanical Properties | High Strength | |
| Marine | Hardware, High Strength | Corrosion Resistance | Corrosion Resistance |
| Hardware, High Strength | Forming Characteristics | Formability | |
| Hardware, High Strength | Mechanical Properties | Ductility | |
| Hardware, High Strength | Mechanical Properties | High Strength | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance | |
| Pump Parts | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Pump Parts | Forming Characteristics | Formability | |
| Pump Parts | Mechanical Properties | High Strength |
Applicable Specifications
Corrosion Properties