Find suppliers for this alloy
C66908
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | Mn | |
|
(1) Not including Ag. (2) Cu + Sum of Named Elements 99.5% min. |
||||||||
| Min (%) | 6.0 | 0.01 | 0.01 | 4.0 | ||||
| Max (%) | Rem | 0.05 | 0.50 | 9.0 | 2.0 | 3.5 | 0.25 | 7.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| Flat Products & Tubing | 1/2 Hard | H02 | |
| 1/4 Hard | H01 |
68 Typ |
|
| Annealed | O61 |
61 Typ |
|
| Hard | H04 |
89 Typ |
|
| (1)As Annealed | |
| Densitylb/cu in. at 68°F | 0.307 |
|---|---|
| Specific Gravity | 8.5 |
| Electrical Conductivity% IACS at 68°F | 5 (1) |
| Modulus of Elasticity in Tensionksi | 15000 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Excellent |
| Coated Metal Arc Welding | Good |
| Spot Weld | Excellent |
| Seam Weld | Excellent |
| Butt Weld | Excellent |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 60 |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties