C66920
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Ni(3) | C | Mn | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) Not including Ag. (3) Ni value includes Co. |
||||||||||
| Min (%) | 66.0 | 10.0 | 3.0 | 12.0 | .10 | |||||
| Max (%) | 70.0 | .09 | 14.0 | .6 | 6.0 | .10 | 16.0 | .25 | 1.0 | .05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Rod | Hard | H04 |
102.4 Typ |
93.1 Typ |
1.0 Typ |
98 Typ |
| Hard and Stress Relieved | HR04 |
64.8 Typ |
30.7 Typ |
30 Typ |
58 Typ |
|
| Melting Point - Liquidus°F | 1771 |
|---|---|
| Melting Point - Solidus°F | 1550 |
| Densitylb/cu in. at 68°F | 0.292 |
| Specific Gravity | 8.1 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.0951 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties