Find suppliers for this alloy
C66925
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | Co | Mn | |
|
(1) Not including Ag. (2) Cu + Sum of Named Elements 99.5% min. |
|||||||||
| Min (%) | 17.0 | 0.01 | 8.0 | ||||||
| Max (%) | Rem | 0.05 | 0.50 | 21.0 | 0.50 | 3.5 | 0.25 | 0.01 | 11.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| Flat Products & Tubing | 1/2 Hard | H02 |
84 Typ |
| 1/4 Hard | H01 |
72 Typ |
|
| Anneal | ANNEAL |
64 Typ |
|
| Extra Hard | H06 |
110 Typ |
|
| Hard | H04 |
94 Typ |
|
| Spring | H08 |
121 Typ |
|
| (1)As Annealed | |
| Densitylb/cu in. at 68°F | 0.295 |
|---|---|
| Specific Gravity | 8.16 |
| Electrical Conductivity% IACS at 68°F | 4.5 (1) |
| Modulus of Elasticity in Tensionksi | 15000 |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Good |
| Seam Weld | Excellent |
| Butt Weld | Excellent |
| Capacity for Being Cold Worked | Good |
| Capacity for Being Hot Formed | Good |
| Machinability Rating | 60 |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties