| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Zn | Fe | Al | Mn | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||
| Min (%) | 14.0 | 1.0 | 14.0 | |||
| Max (%) | Rem | 0.01 | 15.0 | 0.50 | 1.5 | 15.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Flat Products | 1/2 Hard | H02 |
65 Typ |
29 Typ |
35 Typ |
95 Typ |
| 1/2 Hard | H02 |
75 Typ |
36 Typ |
30 Typ |
120 Typ |
|
| Electrical Conductivity% IACS at 68°F | 3.4 |
|---|---|
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 20 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 12.5 |
| Modulus of Elasticity in Tensionksi | 18100 |
| Technique | Suitability |
|---|---|
| Soldering | Not Recommended |
| Brazing | Not Recommended |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Good |
| Spot Weld | Good |
| Butt Weld | Good |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties