Find suppliers for this alloyC67000
Chemical Composition
Element
Cu(1,2)PbSnZnFeAlMn
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag.
Min (%)63.02.03.02.5
Max (%)68.00.200.50Rem4.06.05.0
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Melting Point - Liquidus°F1652
Densitylb/cu in. at 68°F0.286
Specific Gravity7.92
Electrical Conductivity% IACS at 68°F22
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F57
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)11.9
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialForgingsCorrosion ResistanceCorrosion Resistance
ForgingsFriction & Wear PropertiesWearability
ForgingsMechanical PropertiesFatigue Resistance
ForgingsMechanical PropertiesHigh Strength
Applicable Specifications
Form Sub-Form System Standard Description
BarASTMB138/B138MMANGANESE BRONZE ROD, BAR AND SHAPES
SAEJ461WROUGHT AND CAST COPPER ALLOYS
SAEJ463WROUGHT COPPER AND COPPER ALLOYS
ForgingsForgingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
ForgingsSAEJ463WROUGHT COPPER AND COPPER ALLOYS
RodASTMB138/B138MMANGANESE BRONZE ROD, BAR AND SHAPES
SAEJ461WROUGHT AND CAST COPPER ALLOYS
SAEJ463WROUGHT COPPER AND COPPER ALLOYS
ShapesASTMB138/B138MMANGANESE BRONZE ROD, BAR AND SHAPES
Corrosion Properties

No information available.