C67100
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Mn | |
|
(1) Cu value includes Ag. |
||||||
| Min (%) | 59.0 | 0.15 | 0.50 | 0.20 | 0.05 | |
| Max (%) | 62.0 | 0.35 | 1.0 | Rem | 0.8 | 0.25 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties