C67200
Elements | ||||||
---|---|---|---|---|---|---|
Cu(1) | Pb | Zn | Fe | Ni | Mn | |
(1) Cu value includes Ag. |
||||||
Min (%) | 57.5 | 4.0 | 6.0 | |||
Max (%) | 61.0 | 0.05 | Rem | 0.25 | 6.0 | 8.0 |