Chemical Composition
Element
Cu(1,2)PbSnZnFeNi(3)AlMnSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. (3) Ni value includes Co.
Min (%)58.00.402.00.50
Max (%)63.03.00.30Rem0.500.250.253.51.5
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell B scale
Section Size
(in)
BarExtruded and DrawnH5065   Min
40   Min
11   Min
80   Min
<1.00
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1605
Densitylb/cu in. at 68°F0.3
Specific Gravity8.3
Electrical Conductivity% IACS at 68°F22
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F55
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)11
Modulus of Elasticity in Tensionksi17000
Fabrication Properties
Technique Suitability
Machinability Rating70
Common Fabrication Processes
  • Hot Forming
  • Hot Pressing
  • Machining
Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
FastenersFastenersCorrosion ResistanceCorrosion Resistance
FastenersCorrosion ResistanceStress Corrosion Cracking Resistance
FastenersMachining CharacteristicsMachinability
FastenersMechanical PropertiesHigh Strength
Lead Screw NutsCorrosion ResistanceCorrosion Resistance
Lead Screw NutsMachining CharacteristicsMachinability
Lead Screw NutsMechanical PropertiesHigh Strength
IndustrialBearingsFriction & Wear PropertiesWear Resistance
BearingsMachining CharacteristicsMachinability
BearingsMechanical PropertiesStrength
Bearings, PinsCorrosion ResistanceCorrosion Resistance
Bearings, PinsFriction & Wear PropertiesLow Co-efficient of Friction
Bearings, PinsFriction & Wear PropertiesWear Resistance
Bearings, PinsMachining PropertiesMachinability, Good
Bearings, PinsMechanical PropertiesHigh Strength
BushingsCorrosion ResistanceCorrosion Resistance
BushingsFriction & Wear PropertiesGalling Resistance
BushingsFriction & Wear PropertiesWear Resistance
BushingsMachining CharacteristicsMachinability
Clutch BearingsCorrosion ResistanceCorrosion Resistance
Clutch BearingsFriction & Wear PropertiesLow Co-efficient of Friction
Clutch BearingsFriction & Wear PropertiesWear Resistance
Clutch BearingsMachining PropertiesMachinability, Good
Clutch BearingsMechanical PropertiesHigh Strength
Drive ShaftsCorrosion ResistanceCorrosion Resistance
Drive ShaftsFriction & Wear PropertiesWear Resistance
Drive ShaftsMechanical PropertiesFatigue Strength
Drive ShaftsMechanical PropertiesHigh Strength
Gears and CamsCorrosion ResistanceCorrosion Resistance
Gears and CamsMachining CharacteristicsMachinability
Gears and CamsMechanical PropertiesFatigue Resistance
Gears and CamsMechanical PropertiesHigh Strength
Idler PinsCorrosion ResistanceCorrosion Resistance
Idler PinsMechanical PropertiesFatigue Strength
Idler PinsMechanical PropertiesHigh Strength
Piston HeadsCorrosion ResistanceCorrosion Resistance
Piston HeadsFriction & Wear PropertiesGalling Resistance
Piston HeadsFriction & Wear PropertiesWear Resistance
Piston HeadsMachining PropertiesMachinability, Good
Piston HeadsMechanical PropertiesFatigue Strength
Piston HeadsMechanical PropertiesHigh Strength
Propeller ShaftsCorrosion ResistanceCorrosion Resistance
Propeller ShaftsFriction & Wear PropertiesGalling Resistance
Propeller ShaftsFriction & Wear PropertiesWear Resistance
Propeller ShaftsMachining PropertiesMachinability, Good
Propeller ShaftsMechanical PropertiesHigh Strength
Pump PartsCorrosion ResistanceCorrosion Resistance
Pump PartsFriction & Wear PropertiesGalling Resistance
Pump PartsFriction & Wear PropertiesWear Resistance
Pump PartsMachining PropertiesMachinability, Good
Pump PartsMechanical PropertiesHigh Strength
Seal RingsCorrosion ResistanceCorrosion Resistance
Seal RingsFriction & Wear PropertiesGalling Resistance
Seal RingsFriction & Wear PropertiesWear Resistance
Seal RingsMachining PropertiesMachinability, Good
Seal RingsMechanical PropertiesDuctility
Seal RingsMechanical PropertiesHigh Strength
Shaft BushingsCorrosion ResistanceCorrosion Resistance
Shaft BushingsFriction & Wear PropertiesGalling Resistance
Shaft BushingsFriction & Wear PropertiesLow Co-efficient of Friction
Shaft BushingsFriction & Wear PropertiesWear Resistance
Shaft BushingsMachining PropertiesMachinability, Good
Shaft BushingsMechanical PropertiesHigh Strength
Sleeve BearingsCorrosion ResistanceCorrosion Resistance
Sleeve BearingsFriction & Wear PropertiesGalling Resistance
Sleeve BearingsFriction & Wear PropertiesLow Co-efficient of Friction
Sleeve BearingsFriction & Wear PropertiesWear Resistance
Sleeve BearingsMachining PropertiesMachinability, Good
Sleeve BearingsMechanical PropertiesHigh Strength
SpindlesCorrosion ResistanceCorrosion Resistance
SpindlesMachining PropertiesMachinability, Good
SpindlesMechanical PropertiesDuctility
SpindlesMechanical PropertiesFatigue Strength
SpindlesMechanical PropertiesHigh Strength
Thrust BearingsCorrosion ResistanceCorrosion Resistance
Thrust BearingsFriction & Wear PropertiesLow Co-efficient of Friction
Thrust BearingsFriction & Wear PropertiesWear Resistance
Thrust BearingsMechanical PropertiesHigh Strength
Wear PlatesCorrosion ResistanceCorrosion Resistance
Wear PlatesFriction & Wear PropertiesGalling Resistance
Wear PlatesFriction & Wear PropertiesWear Resistance
Wear PlatesMachining CharacteristicsMachinability
MarineHardwareCorrosion ResistanceCorrosion Resistance
HardwareCorrosion ResistanceCorrosion Resistance to Salt Water
HardwareMachining CharacteristicsMachinability
HardwareMechanical PropertiesHigh Strength
Valve SeatsCorrosion ResistanceCorrosion Resistance to Salt Water
Valve SeatsFriction & Wear PropertiesWear Resistance
Valve SeatsMechanical PropertiesDuctility
Valve SeatsMechanical PropertiesHigh Strength
OtherConnecting RodsCorrosion ResistanceCorrosion Resistance
Connecting RodsFriction & Wear PropertiesWear Resistance
Connecting RodsMachining CharacteristicsMachinability
Connecting RodsMechanical PropertiesFatigue Life
Connecting RodsMechanical PropertiesHigh Strength
Applicable Specifications
Form Sub-Form System Standard Description
BarSAEJ461WROUGHT AND CAST COPPER ALLOYS
SAEJ463WROUGHT COPPER AND COPPER ALLOYS
ForgingsForgingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
ForgingsSAEJ463WROUGHT COPPER AND COPPER ALLOYS
RodSAEJ461WROUGHT AND CAST COPPER ALLOYS
SAEJ463WROUGHT COPPER AND COPPER ALLOYS
ShapesSAEJ461WROUGHT AND CAST COPPER ALLOYS
SAEJ463WROUGHT COPPER AND COPPER ALLOYS
Corrosion Properties

No information available.