Find suppliers for this alloy
C67810
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni | Al | Mn | Si | |
|
(1) Cu value includes Ag. |
|||||||||
| Min (%) | 56.5 | 41.9 | 0.40 | 0.40 | |||||
| Max (%) | 59.5 | 1.0 | 0.50 | Rem | 1.0 | 1.5 | 1.6 | 1.8 | 0.6 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties