Find suppliers for this alloy
C67820
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Al | Mn | |
|
(1) Cu value includes Ag. |
|||||||
| Min (%) | 56.5 | 0.30 | 0.50 | 0.30 | 0.30 | ||
| Max (%) | 59.5 | 0.10 | 1.0 | Rem | 1.2 | 1.2 | 2.0 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties