Find suppliers for this alloy
C68000
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
|||||||||
| Min (%) | 56.0 | 0.75 | 0.25 | 0.20 | 0.01 | 0.04 | |||
| Max (%) | 60.0 | 0.05 | 1.10 | Rem | 1.25 | 0.8 | 0.01 | 0.50 | 0.15 |
Mechanical Properties
| Densitylb/cu in. at 68°F | 0.296 |
|---|---|
| Specific Gravity | 8.19 |
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Welding Rod for Cast Iron | Conductivity (Electrical) | Electrical Conductivity |
| Welding Rod for Cast Iron | Conductivity (Thermal) | Thermal Conductivity | |
| Welding Rod for Cast Iron | Corrosion Resistance | Oxidation Resistance |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod | Welding | AWS | A5.27 | COPPER AND COPPER ALLOY RODS FOR OXYFUEL GAS WELDING | |
| Welding | AWS | A5.15 | WELDING RODS FOR WELDING CAST IRON |
Corrosion Properties