Find suppliers for this alloyC68000
Chemical Composition
Element
Cu(1,2)PbSnZnFeNi(3)AlMnSi
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co.
Min (%)56.00.750.250.200.010.04
Max (%)60.00.051.10Rem1.250.80.010.500.15
Mechanical Properties

No mechanical properties for this alloy

Physical Properties
Densitylb/cu in. at 68°F0.296
Specific Gravity8.19
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialWelding Rod for Cast IronConductivity (Electrical)Electrical Conductivity
Welding Rod for Cast IronConductivity (Thermal)Thermal Conductivity
Welding Rod for Cast IronCorrosion ResistanceOxidation Resistance
Applicable Specifications
Form Application System Standard Description
RodWeldingAWSA5.15WELDING RODS FOR WELDING CAST IRON
WeldingAWSA5.27COPPER AND COPPER ALLOY RODS FOR OXYFUEL GAS WELDING
Corrosion Properties

No information available.