Find suppliers for this alloy
C68100
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Cu value includes Ag. |
||||||||
| Min (%) | 56.0 | 0.75 | 0.25 | 0.01 | 0.04 | |||
| Max (%) | 60.0 | 0.05 | 1.10 | Rem | 1.3 | 0.01 | 0.50 | 0.15 |
Mechanical Properties
Physical Properties
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| Rod | Welding | AWS | A5.27 | COPPER AND COPPER ALLOY RODS FOR OXYFUEL GAS WELDING | |
| Welding | AWS | A5.15 | WELDING RODS FOR WELDING CAST IRON |
Corrosion Properties