Find suppliers for this alloy
C68320
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Al | As | Si | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. (3) Ni value includes Co. |
||||||||||
| Min (%) | 59.0 | 0.02 | 0.05 | |||||||
| Max (%) | 65.0 | 0.25 | 0.50 | Rem | 0.30 | 0.20 | 0.20 | 0.09 | 0.16 | 0.50 |
| Form | Temper | Temper Code | Elongation (%) |
Rockwell B scale | Shear Strength (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Ultimate Tensile Strength in Shear (ksi) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Die Forging | As Hot Forged - Air Cooled | M10 | 30 Min 60 Max |
70 Min 105 Max |
34.8 Typ |
293 Typ | 49.3 Min 53.7 Typ 69.6 Max |
| Melting Point - Liquidus°F | 1633 |
|---|---|
| Densitylb/cu in. at 68°F | 0.304 |
| Specific Gravity | 8.41 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 56.4 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 11.11 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 11.2 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.59 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.092 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Excellent |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Fair |
| Seam Weld | Fair |
| Butt Weld | Poor |
| Capacity for Being Cold Worked | Fair |
| Capacity for Being Hot Formed | Good |
| Forgeability Rating | 75 |
| Machinability Rating | 70 |
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Enviornmentaly friendly Faucets and Plumbing Components | ||
| Valve Bodies, Faucets, Plumbing Components |
Applicable Specifications