Find suppliers for this alloy
C68330
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
||||||||||
| Min (%) | 58.5 | 0.10 | 0.10 | |||||||
| Max (%) | 60.5 | 0.100 | 0.20 | Rem | 0.20 | 0.20 | 0.20 | 0.05 | 0.05 | 0.3 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Forgings |
76.9 Typ |
58.0 Typ |
20 Typ |
||
| Rod & Bar | 1/2 Hard | H02 |
76.9 Typ |
58.0 Typ |
19 Typ |
| Wire | 1/2 Hard | H02 |
76.9 Typ |
58.0 Typ |
20 Typ |
| Densitylb/cu in. at 68°F | 0.3 |
|---|---|
| Specific Gravity | 7.21 |
| Electrical Conductivity% IACS at 68°F | 23 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 60 |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Fair |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Spot Weld | Fair |
| Seam Weld | Fair |
| Butt Weld | Fair |
| Capacity for Being Cold Worked | Fair |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 100 |
| Machinability Rating | 90 |
Common Fabrication Processes
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Connectors | Lead Free | Machinability, Good |
| Industrial | Plumbing Parts |
Applicable Specifications
Corrosion Properties